Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 9.40 µm/m-°C

@Temperature 20.0 °C
5.22 µin/in-°F

@Temperature 68.0 °F
Haveg 41N Phenolic; Silicate Reinforced Ablative Material