Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.31 GPa | 1350 ksi | ASTM D638 |
Quadrant EPP Ketron® CM 1030HT PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | ISO 527 |
Nilit FRIANYL B63 HS-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2300 PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2300R PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 420HP PBT 30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420.. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp MF0069S PP (Asia Pacific) LNP* Thermocomp* MF0069S is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant, Heat Stabi.. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-kon DX96690 PC LNP STAT-KON* DX96690 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the America.. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East) Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | dry; ISO 527-1/-2 |
DSM Akulon® N24-G6 PA6-GF30 30% Glass Reinforced |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GVZ 30 HWCP 30% Glass Fiber Z-Qualities Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 GF6 POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | ASTM D638 |
BLUESTAR 201-G20202 PBT, 20% Glass Filled Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Modulus | 9.30 GPa | 1350 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Verton PV007SV_YW8D151 PA 6 Preliminary data for 35% long fiber single pellet color filled PA6This data was supplied by SABIC-IP for the Americas region. |