Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.39 µm/m-°C @Temperature 500 °C |
5.22 µin/in-°F @Temperature 932 °F |
|
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m.. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 500 °C |
5.22 µin/in-°F @Temperature 68.0 - 932 °F |
|
Misumi Machinable SiO2-MgO Ceramic Information provided by MISUMI Corporation. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 °C |
5.22 µin/in-°F @Temperature 68.0 °F |
in x- and y-directions |
Haveg 41N Phenolic; Silicate Reinforced Ablative Material A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers converted to a permanent thermoset state under heat and pressure. It is designed for abla.. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SF10 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SF14 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott P-SF8 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 300 °C |
5.22 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott UG5 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 300 °C |
5.22 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-KZFS8 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Fastener Stock Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of fastener stock; more specific form/thickness entries are also available in MatWeb.Industry Specifications: .. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of rod; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aeros.. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G; other specific form/thickness entries .. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of sheet; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aero.. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265 Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265; other specific form/thickness entries a.. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >0.500-1.000 in, STD, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >0.500-1.000 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i.. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >1.000-1.500 in, STD, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >1.000-1.500 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i.. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G; other specific form/thickness entries are .. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V-0.1Ru; ASTM Grade 29) Medium To High Strength General-Purpose Alloy. Property data below are typical of Timet® 6-4 ELI (without Ru). The 0.1 Ru ELI variant is used for enhanced corrosion resistance.Data provided by TI.. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; Medium To High Strength General-Purpose Alloy Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A .. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 1.75 - 2.50 in Rod or Thickness; Per ASTM F136) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 2.50 - 4.00 in Rod or Thickness; Per ASTM F136) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Solution Treated; 0.025 - 1.000 in Sheet and Plate; Per ASTM B265) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 20.0 - 425 °C |
5.22 µin/in-°F @Temperature 68.0 - 797 °F |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >1.500-2.000 in, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >1.500-2.000 in, Per Mil-T-9047G; other specific form/thickness entries are .. |
|||
CTE, linear | 9.40 µm/m-°C @Temperature 25.0 - 1001 °C |
5.22 µin/in-°F @Temperature 77.0 - 1834 °F |
|
CeramTec 645 Steatite (MgO-SiO2) Te value is 810°C. Hasselman Thermal Shock value is 600 K.Data provided by CeramTec North America. |