Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.320 W/m-K @Temperature 90.0 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | In-Plane; ASTM E1461 |
Victrex® APTIV® 1000-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline APTIV PEEK 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTI.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 23.0 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Along flow; ISO/CD 22007-4 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 90G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, .. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | |
Haveg 41N Phenolic; Silicate Reinforced Ablative Material A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers converted to a permanent thermoset state under heat and pressure. It is designed for abla.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2312EPR PEI 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | ISO 8302 |
Solvay Specialty Polymers Ryton® R-4-280BL Polyphenylene Sulfide (PPS), Glass Fiber Ryton® R-4-280BL 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | ISO 8302 |
Solvay Specialty Polymers Ryton® R-4-280NA Polyphenylene Sulfide (PPS), Glass Fiber Ryton® R-4-280NA 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Valox® VX8532 PBT+PET (Europe-Africa-Middle East) VALOX VX8532 is a 30% glassfiber reinforced, non blooming, flame retardant PBT+PET blend with excellent surface appearance and good ultrasonic weldability properties.This data was supplied by SABIC-.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | ASTM C-518 |
Sumitomo Bakelite North America RX® 1366FR-P Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG-F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Thermal Conductivity | 0.320 W/m-K @Temperature 100 °C |
2.22 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1225 |
Arlon AD260A PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Low Loss PTFE and Ceramic Filled Composite Dielectric Constant (2.60)Low Dielectric Loss (Loss Tangent)Low Profile Copper (lower conductive losses)Low Z-d.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | |
Arlon AD300A Glass, PTFE and Micro-Dispersed Ceramic Lower Loss and Improved Performance over Traditional AD Series.Information provided by Arlon Materials for Electronics (MED). |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | |
Arlon R30370A008 0.008" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3L BK00464 PA6 (Conditioned) Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall .. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur® B 4406 G6 30% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3L BK00464 PA6 (Dry) Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall .. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3L PA6 (Conditioned) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
Thermal Conductivity | 0.320 W/m-K | 2.22 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |