Material Notes:
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ready-to-process Ampersint® Map powder.
Physical Properties Metric English Comments
Density 8.15 g/cc
0.294 lb/in³
Porosity <= 3 %
<= 3 %
sintered
Mechanical Properties Metric English Comments
Tensile Strength, Yield 650 MPa

@Temperature 600 °C
94300 psi

@Temperature 1110 °F
700 MPa

@Temperature 400 °C
102000 psi

@Temperature 752 °F
710 MPa

@Temperature 200 °C
103000 psi

@Temperature 392 °F
Component Elements Properties Metric English Comments
Carbon, C 1.0 %
1.0 %
Cobalt, Co 49 - 51 %
49 - 51 %
Iron, Fe 49 - 51 %
49 - 51 %
Electrical Properties Metric English Comments
Magnetic Permeability 7577
7577
Magnetic Coercive Force, Hc 1.696 Oe
1.696 Oe
Magnetic Saturation Flux Density, Bmax 22000 Gauss
22000 Gauss