Mechanical Properties Metric English Comments
Tensile Strength, Yield 650 MPa

@Strain 1.00 %,
Temperature -196 °C
94300 psi

@Strain 1.00 %,
Temperature -321 °F
EN min.; EN 10002-5
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 650 MPa

@Strain 0.200 %
94300 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
Outokumpu 4313 Martensitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Tensile Strength, Yield 650 MPa

@Temperature 600 °C
94300 psi

@Temperature 1110 °F
H.C. Starck Ampersint® MAP FeCoNi 40/20/40 For Hardmetals
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Tensile Strength, Yield 650 MPa

@Temperature 600 °C
94300 psi

@Temperature 1110 °F
H.C. Starck Ampersint® MAP FeCoNi 70/10/20 For Hardmetals
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Tensile Strength, Yield 650 MPa

@Temperature 600 °C
94300 psi

@Temperature 1110 °F
H.C. Starck Ampersint® MAP FeNi 50/50 For Hardmetals
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Tensile Strength, Yield 650 MPa

@Temperature 600 °C
94300 psi

@Temperature 1110 °F
H.C. Starck Ampersint® MAP FeNi 50/50 For Soft Magnets
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Tensile Strength, Yield 650 MPa

@Temperature 600 °C
94300 psi

@Temperature 1110 °F
H.C. Starck Ampersint® MAP FeCo 50/50 For Soft Magnets
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Tensile Strength, Yield 650 MPa

@Temperature 25.0 °C,
Time 45700 sec
94300 psi

@Temperature 77.0 °F,
Time 12.7 hour
As Welded, Solution Annealed, and Aged; Weld/Weld Fracture; 0.2% Offset
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Tensile Strength, Yield >= 650 MPa

@Thickness >=65.0 mm
>= 94300 psi

@Thickness >=2.56 in
ThyssenKrupp N-A-XTRA® M 700 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..