Polymer Property : Magnetic Saturation Flux Density, Bmax = 22000 Gauss Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Magnetic Saturation Flux Density, Bmax 22000 Gauss
22000 Gauss
H.C. Starck Ampersint® MAP FeCo 50/50 For Soft Magnets
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..