Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 710 MPa @Temperature 200 °C |
103000 psi @Temperature 392 °F |
|
H.C. Starck Ampersint® MAP FeCoNi 40/20/40 For Hardmetals High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Tensile Strength, Yield | 710 MPa @Temperature 200 °C |
103000 psi @Temperature 392 °F |
|
H.C. Starck Ampersint® MAP FeCoNi 70/10/20 For Hardmetals High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Tensile Strength, Yield | 710 MPa @Temperature 200 °C |
103000 psi @Temperature 392 °F |
|
H.C. Starck Ampersint® MAP FeNi 50/50 For Hardmetals High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Tensile Strength, Yield | 710 MPa @Temperature 200 °C |
103000 psi @Temperature 392 °F |
|
H.C. Starck Ampersint® MAP FeNi 50/50 For Soft Magnets High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Tensile Strength, Yield | 710 MPa @Temperature 200 °C |
103000 psi @Temperature 392 °F |
|
H.C. Starck Ampersint® MAP FeCo 50/50 For Soft Magnets High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Tensile Strength, Yield | 710 MPa @Strain 0.200 %, Temperature 100 °C |
103000 psi @Strain 0.200 %, Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Yield | 710 MPa @Temperature -55.0 °C |
103000 psi @Temperature -67.0 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |