Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 102000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 700 MPa

@Strain 0.200 %
102000 psi

@Strain 0.200 %
Outokumpu Typical, Quenched & Tempered Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4313 Martensitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Tensile Strength, Yield 700 MPa

@Strain 1.00 %,
Temperature -196 °C
102000 psi

@Strain 1.00 %,
Temperature -321 °F
EN min.; EN 10002-5
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 700 MPa

@Strain 1.00 %,
Temperature -196 °C
102000 psi

@Strain 1.00 %,
Temperature -321 °F
EN min.; EN 10002-5
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms.
Tensile Strength, Yield 700 MPa

@Temperature 400 °C
102000 psi

@Temperature 752 °F
H.C. Starck Ampersint® MAP FeCoNi 40/20/40 For Hardmetals
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Tensile Strength, Yield 700 MPa

@Temperature 400 °C
102000 psi

@Temperature 752 °F
H.C. Starck Ampersint® MAP FeCoNi 70/10/20 For Hardmetals
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Tensile Strength, Yield 700 MPa

@Temperature 400 °C
102000 psi

@Temperature 752 °F
H.C. Starck Ampersint® MAP FeNi 50/50 For Hardmetals
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Tensile Strength, Yield 700 MPa

@Temperature 400 °C
102000 psi

@Temperature 752 °F
H.C. Starck Ampersint® MAP FeNi 50/50 For Soft Magnets
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Tensile Strength, Yield 700 MPa

@Temperature 400 °C
102000 psi

@Temperature 752 °F
H.C. Starck Ampersint® MAP FeCo 50/50 For Soft Magnets
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Tensile Strength, Yield 700 MPa

@Strain 0.200 %,
Temperature 700 °C
102000 psi

@Strain 0.200 %,
Temperature 1290 °F
Special Metals UDIMET® alloy 520 Superalloy
UDIMET® alloy 520 is a precipitation-hardenable nickel base superalloy with an exceptional combination of high-temperature mechanical properties, corrosion resistance and forgeability characteris..
Tensile Strength, Yield >= 700 MPa

@Thickness 65.0 mm
>= 102000 psi

@Thickness 2.56 in
ThyssenKrupp N-A-XTRA® M 700 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield 702 MPa

@Strain 0.200 %
102000 psi

@Strain 0.200 %
9.8% Cold Work
AK Steel NITRONIC® 19-D Duplex Stainless Steel
AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}), good drawing and welding characteristi..
Tensile Strength, Yield 702 MPa

@Strain 0.200 %
102000 psi

@Strain 0.200 %
Typical for Plate, 1/4-Hard, Longitudinal, 0.25"
AK Steel NITRONIC® 30 Austenitic Stainless Steel
AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi..
Copyright © lookpolymers.com All Rights Reserved