Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Saturation Flux Density, Bmax | 22000 Gauss | 22000 Gauss | |
H.C. Starck Ampersint® MAP FeCo 50/50 For Soft Magnets High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |