Gwent Electronic Materials C2030304D2 Aluminum Ink

Category Fluid , Metal , Electronic/Magnetic Alloy , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2030304D2 Aluminum Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
C2030304D2 is designed as a screen printing ink for termination of Barium Titanate based PTC devices.This Ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 64 - 66 %
64 - 66 %
Particle Size <= 8.0 µm
<= 8.0 µm
Main Break; Fineness of Grind
<= 20 µm
<= 20 µm
3rd Streak; Fineness of Grind
Viscosity 4100 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
4100 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer with the PK1.1°
Storage Temperature 25.0 °C
77.0 °F
Processing Properties Metric English Comments
Processing Temperature 60.0 °C
140 °F
Dry Time 0.167 - 0.25 hour
0.167 - 0.25 hour
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Printing Mesh counts/inch 180 to 340
stainless steel or polyester screens