Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 0.167 - 0.25 hour | 0.167 - 0.25 hour | |
Gwent Electronic Materials C2030304D2 Aluminum Ink C2030304D2 is designed as a screen printing ink for termination of Barium Titanate based PTC devices.This Ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen .. |