Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 60.0 °C | 140 °F | Curing Agent Temperature |
Northstar Polymers MSB-M25B Microcellular Foam based on High Performance Polyester Polyurethane This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste.. |
|||
Processing Temperature | 60.0 °C | 140 °F | Curing Agent Temperature |
Northstar Polymers MSB-M25F Microcellular Foam based on High Performance Polyester Polyurethane This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste.. |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Gwent Electronic Materials D2030210D1 Polymer Dielectric This material is a black colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode.. |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Gwent Electronic Materials D50706D2 Polymer Dielectric This material is a cream colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode.. |
|||
Processing Temperature | >= 60.0 °C | >= 140 °F | Activation Temperature; EN-12961 |
Lubrizol Advanced Materials Pearlstick® 48-60/03 Linear Thermoplastic Polyurethane Elastomer Pearlstick 48-60/03 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low-medium thermoplasticity level, available as pellets.Solubility: Pearlstick 48-60.. |
|||
Processing Temperature | >= 60.0 °C | >= 140 °F | Activation Temperature; EN-12961 |
Lubrizol Advanced Materials Pearlstick® 48-60/25 Linear Thermoplastic Polyurethane Elastomer Pearlstick 48-60/25 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low-medium thermoplasticity level, available as pellets.Solubility: Pearlstick 48-60.. |
|||
Processing Temperature | 60.0 °C | 140 °F | EN-12961 |
Lubrizol Advanced Materials Pearlstick® D40-70/14 Linear Thermoplastic Polyurethane Pearlstick D40-70/14 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. .. |
|||
Processing Temperature | 60.0 °C | 140 °F | EN-12961 |
Lubrizol Advanced Materials Pearlstick® D40-70/18 Linear Thermoplastic Polyurethane Pearlstick D40-70/18 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. .. |
|||
Processing Temperature | 60.0 - 65.0 °C | 140 - 149 °F | Temperature setting, B component |
Taiwan PU Corporation TPL-THANE 5085-A/B High Pressure Urethane Spraying Elastomer 5085-A is a high reactivity polyethamine content extender. 5085-B is a methylene diphenyklene dissocyanate(MDI). They make up the third generation high pressure urethane spraying elastomer. It ha.. |
|||
Processing Temperature | 60.0 °C | 140 °F | non show side |
Lubrizol Telene 1620 A/BK Dicyclopentadiene (DCPD) Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® resu.. |
|||
Processing Temperature | 60.0 °C | 140 °F | hopper drying |
Borealis LE0592 Polyethylene LE0592 is a crosslinkable black polyethylene compound, specially designed for bonded semi conductive screen applications. Applications: LE0592 is intended for semi conductive applications in XLPE m.. |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Hopper |
Eurostar Staramide ALY430A PA66, Glass Fiber Reinforced, Injection Molding Staramide ALY430A is a Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Processing Temperature | 60.0 - 240 °C | 140 - 464 °F | Injection |
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Processing Temperature | 60.0 - 240 °C | 140 - 464 °F | Injection |
Alliance Polymers Viprene™ G45D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Processing Temperature | 60.0 °C | 140 °F | hopper drying; 4h |
Borealis LE7710 Polyethylene Compound, Semiconductive, Thermoplastic LE7710 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7710 is intended for semiconductive applications in medium voltage .. |
|||
Processing Temperature | 60.0 °C | 140 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 46-73/15 Polyester based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: Shoe, OthersInformation provided by Merquinsa |
|||
Processing Temperature | 60.0 °C | 140 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 46-73/27 Polyester based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: ShoeInformation provided by Merquinsa |
|||
Processing Temperature | 60.0 °C | 140 °F | |
Gwent Electronic Materials C2030304D2 Aluminum Ink C2030304D2 is designed as a screen printing ink for termination of Barium Titanate based PTC devices.This Ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen .. |