Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 3.00 Month | 3.00 Month | From date of Manufacture |
Parker Chomerics THERM-A-FORM T646 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials C10903P14 Carbon/Graphite Ink Carbon Graphite Ink is used for screen printing working electrodes. This is a carbon graphite ink, which has been optimized to give superior electrochemical performance with good reversibility when.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials C2000808D2 Silver Backlight Ink Silver Ink C2000808D2 is a high resistance ink designed for use as the heating bars and tracks on automobile backlights and other circuits on glass. It has dark color when printed and fired on floa.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials C2051014P10 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. Applications in medical diagnostics, environmentalScreen Printing Equipment: semi-automatic, manualScreen Types: polye.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials D50706P3 Polymer Dielectric This material is a blue colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode... |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials G2020520D1 Gold Metallo-Organic Ink This is a screen printing ink designed to act as a working electrode when fired onto alumina substrates. This unique MO formulation gives a fired thickness in the order of 0.2 to 0.3 microns. This.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials C2031105D2 Palladium Ink Palladium Ink C2031105D2 is an ink formulated for screen printing for use on Fuel Cells. It is suitable for application onto Solid Oxide Fuel Cells.The ink has been made at a ready to use viscosity.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | with proper storage |
Stanelco Bioplast® Wrap 100 Biodegradable Plastic Bioplast Wrap 100 is a plasticiser-free thermoplastic material which allows the production of films with coated paper-like properties. Wrap 100 is an excellent, eco-friendly alternative to laminated.. |
|||
Shelf Life | 3.00 - 6.00 Month @Temperature 4.44 - 7.22 °C |
3.00 - 6.00 Month @Temperature 40.0 - 45.0 °F |
in original, unopened containers |
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | syringe |
Master Bond EP79 Two Component, Silver Coated, Nickel Filled Conductive Epoxy Master Bond Polymer System EP79 is a two component, silver coated, nickel filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or .. |
|||
Shelf Life | 3.00 Month | 3.00 Month | at 25°C |
Tipco Tipwood® 50 EX 50EX Description: Tipwood® is a Wood-Fiber Reinforced, Heat Stabilized Polypropylene Compound specially developed by Tipco for Automobile Interiors and Appliance Fascia Applications.Features: Environmen.. |
|||
Shelf Life | 3.00 Month @Temperature -40.0 °C |
3.00 Month @Temperature -40.0 °F |
|
Loctite® 3565 High performance epoxy, high Tg and low CTE High Tg Underfill COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Shelf Life | 3.00 - 6.00 Month @Temperature 23.9 °C |
3.00 - 6.00 Month @Temperature 75.0 °F |
in original unopened container |
Master Bond EP36AN One Part, Toughened, B-Stage Epoxy Description: Master Bond EP36AN is a unique one component, high performance epoxy for bonding, encapsulation, potting and coating featuring thermal conductivity, electrical insulation and high tempe.. |
|||
Shelf Life | 3.00 Month @Temperature -40.0 °C |
3.00 Month @Temperature -40.0 °F |
|
Loctite® 3534 Glob Top Encapsulant COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Dow Corning HV 1760/80 SILICONE RUBBER NATURAL 80 Shore hardness high consistency silicone rubber with fast cure system and excellent tracking and erosion resistanceInformation provided by Dow Corning |
|||
Shelf Life | 3.00 Month | 3.00 Month | Moisture absorption after extended storage |
Fainplast Compounds EVAtech 805S Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month | 3.00 Month | Moisture absorption after extended storage |
Fainplast Compounds EVAtech 807I Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFC 0115/1 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding for tandem extrusion onlyInformation provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFX 505 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; InsulationInformation provided by Fainplast Com.. |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFX 505/2 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; InsulationInformation provided by Fainplast Com.. |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFX 509 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Insulation for solar cablesInformation provided by Fainpla.. |
|||
Shelf Life | 3.00 Month @Temperature 25.0 °C |
3.00 Month @Temperature 77.0 °F |
|
Epoxy Technology EPO-TEK® H31 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31 is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electronic.. |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HF 045/16M Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, low shrinkageInformation provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month @Temperature 4.44 °C |
3.00 Month @Temperature 40.0 °F |
From date of manufacture |
Arlon R33670N004 0.004" (0.102 mm) Uncured Silicone Rubber with K2030 PEN Film Substrate Design/Construction:Side 1: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Inf.. |
|||
Shelf Life | 3.00 Month @Temperature 4.44 °C |
3.00 Month @Temperature 40.0 °F |
From date of manufacture |
Arlon R35798R013 0.013" (0.330 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 Fiberglass Side 2: Uncured Silicone RubberThis data represents typic.. |
|||
Shelf Life | 3.00 Month @Temperature 7.22 °C |
3.00 Month @Temperature 45.0 °F |
From date of manufacture |
Arlon R38020B020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material. The data should not be used to wr.. |
|||
Shelf Life | 3.00 Month @Temperature 7.22 °C |
3.00 Month @Temperature 45.0 °F |
From date of manufacture |
Arlon 32400N030 0.030" (0.762 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PET Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for the productio.. |
|||
Shelf Life | 3.00 - 6.00 Month @Temperature 23.9 °C |
3.00 - 6.00 Month @Temperature 75.0 °F |
in original unopened containers |
Master Bond Supreme 10HTND-3 Non-Drip Epoxy Resists High Temperatures Description: Master Bond Supreme 10HTND-3 features a blend of performance properties including both high shear and peel strengths along with a totally non-drip application feature. This one componen.. |