Material Notes:
Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.15 - 1.25 g/cc
0.0415 - 0.0452 lb/in³
After drying at 110°C
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 5.00 - 9.00 MPa

@Temperature 1000 °C
725 - 1310 psi

@Temperature 1830 °F
Cold Crushing Strength
8.00 - 12.0 MPa

@Temperature 100 °C
1160 - 1740 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.230 - 0.330 W/m-K

@Temperature 100 °C
1.60 - 2.29 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.280 - 0.380 W/m-K

@Temperature 600 °C
1.94 - 2.64 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.320 - 0.420 W/m-K

@Temperature 1000 °C
2.22 - 2.91 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1350 °C
2460 °F
Shrinkage -0.600 - 0.400 %

@Temperature 1000 °C
-0.600 - 0.400 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 40 %
40 %
Fe2O3 <= 1.0 %
<= 1.0 %
SiO2 40 %
40 %
Descriptive Properties Value Comments
ASTM Classification Q
Material Consumption per 1 m3 1150 kg
Mixing Water 30-35 liters
per 100 kgs dry material