Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 5.00 - 9.00 MPa @Temperature 1000 °C |
725 - 1310 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 135 RL C Refractory Insulating Castable Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast .. |
|||
Compressive Strength | 5.00 - 9.00 MPa @Temperature 1000 °C |
725 - 1310 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE MW Refractory Insulating Castable Description: Golite MW (medium weight) is composed of a light weight refractory aggregate plus several additives to improve the mechanical properties.Remarks: These values apply to cast products. Al.. |