Compressive Strength 8.00 MPa

@Strain 1 %
1160 psi

@Strain 1 %
ISO 604
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data)
Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su..
Compressive Strength 8.00 - 12.0 MPa

@Temperature 100 °C
1160 - 1740 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 135 Refractory Insulating Castable
Description: Golite 135 can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning vari..
Compressive Strength 8.00 - 12.0 MPa

@Temperature 100 °C
1160 - 1740 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 135 RL C Refractory Insulating Castable
Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast ..
Compressive Strength 8.00 - 14.0 MPa

@Temperature 1400 °C
1160 - 2030 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable
Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information..
Compressive Strength 8.00 - 12.0 MPa

@Temperature 100 °C
1160 - 1740 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE MW Refractory Insulating Castable
Description: Golite MW (medium weight) is composed of a light weight refractory aggregate plus several additives to improve the mechanical properties.Remarks: These values apply to cast products. Al..
Compressive Strength 8.00 - 12.0 MPa

@Temperature 1260 °C
1160 - 1740 psi

@Temperature 2300 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 135 GM Refractory Insulating Castable
Description: This gunning material can be used in direct contact with open fire and has a high strength.Remarks: These values were obtained from cast samples. These values apply to cast products.Inf..
Compressive Strength 8.00 - 14.0 MPa

@Temperature 1370 °C
1160 - 2030 psi

@Temperature 2500 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable
Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere...