Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 8.00 MPa @Strain 1 % |
1160 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Compressive Strength | 8.00 - 12.0 MPa @Temperature 100 °C |
1160 - 1740 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 135 Refractory Insulating Castable Description: Golite 135 can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning vari.. |
|||
Compressive Strength | 8.00 - 12.0 MPa @Temperature 100 °C |
1160 - 1740 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 135 RL C Refractory Insulating Castable Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast .. |
|||
Compressive Strength | 8.00 - 14.0 MPa @Temperature 1400 °C |
1160 - 2030 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information.. |
|||
Compressive Strength | 8.00 - 12.0 MPa @Temperature 100 °C |
1160 - 1740 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE MW Refractory Insulating Castable Description: Golite MW (medium weight) is composed of a light weight refractory aggregate plus several additives to improve the mechanical properties.Remarks: These values apply to cast products. Al.. |
|||
Compressive Strength | 8.00 - 12.0 MPa @Temperature 1260 °C |
1160 - 1740 psi @Temperature 2300 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 135 GM Refractory Insulating Castable Description: This gunning material can be used in direct contact with open fire and has a high strength.Remarks: These values were obtained from cast samples. These values apply to cast products.Inf.. |
|||
Compressive Strength | 8.00 - 14.0 MPa @Temperature 1370 °C |
1160 - 2030 psi @Temperature 2500 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere... |