Gouda Vuurvast FLUCON 180 Dense Self Flowing Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name FLUCON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast FLUCON 180 Dense Self Flowing Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Flucon 180 is a self flowing castable based on white fused Alumina. This castable is applied at severe thermal conditions and or severe slag attack.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 3.15 - 3.25 g/cc
0.114 - 0.117 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 70.0 - 90.0 MPa

@Temperature 100 °C
10200 - 13100 psi

@Temperature 212 °F
Cold Crushing Strength
185 - 215 MPa

@Temperature 1600 °C
26800 - 31200 psi

@Temperature 2910 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.85 - 2.05 W/m-K

@Temperature 600 °C
12.8 - 14.2 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.90 - 2.10 W/m-K

@Temperature 100 °C
13.2 - 14.6 BTU-in/hr-ft²-°F

@Temperature 212 °F
2.00 - 2.20 W/m-K

@Temperature 1600 °C
13.9 - 15.3 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Maximum Service Temperature, Air 1800 °C
3270 °F
Shrinkage -0.500 - 0.500 %

@Temperature 1600 °C
-0.500 - 0.500 %

@Temperature 2910 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 98 %
98 %
CaO 1.5 %
1.5 %
Fe2O3 <= 0.20 %
<= 0.20 %
SiO2 <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 3150 kg
Mixing Water 3.5-4 liters
per 100 kgs dry material