Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.84 W/m-K @Temperature 1093 °C |
12.8 BTU-in/hr-ft²-°F @Temperature 1999 °F |
|
Pyrotek Pyrocast PT-190 Refractory Cast Parts Pyrocast PT-190 is an extremely dense alumina based refractory. It is best suited for applications where high velocity metal erosion potential is a problem, due to its strength and abrasion resista.. |
|||
Thermal Conductivity | 1.85 - 2.05 W/m-K @Temperature 100 °C |
12.8 - 14.2 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 150 GZ (R) Dense Vibrating Refractory Castable Description: Vibron 150 GZ (R) is a low cement castable based on sintered South-American bauxite. The addition of zircon oxide in this product makes it suitable for areas under heavy chemical attack.. |
|||
Thermal Conductivity | 1.85 - 2.05 W/m-K @Temperature 600 °C |
12.8 - 14.2 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 150 GZ (R) Dense Vibrating Refractory Castable Description: Vibron 150 GZ (R) is a low cement castable based on sintered South-American bauxite. The addition of zircon oxide in this product makes it suitable for areas under heavy chemical attack.. |
|||
Thermal Conductivity | 1.85 W/m-K @Temperature 700 °C |
12.8 BTU-in/hr-ft²-°F @Temperature 1290 °F |
Thru-thickness |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.85 W/m-K @Temperature 500 °C |
12.8 BTU-in/hr-ft²-°F @Temperature 932 °F |
Fill direction |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.85 W/m-K @Temperature 500 °C |
12.8 BTU-in/hr-ft²-°F @Temperature 932 °F |
Warp direction |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.85 - 2.05 W/m-K @Temperature 600 °C |
12.8 - 14.2 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast FLUCON 180 Dense Self Flowing Refractory Castable Description: Flucon 180 is a self flowing castable based on white fused Alumina. This castable is applied at severe thermal conditions and or severe slag attack.Remarks: These values apply to cast p.. |