Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 3.15 - 3.25 g/cc | 0.114 - 0.117 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 180 Dense Vibrating Refractory Castable Description: Vibron 180 is a low cement castable with an alumina bond. The material is supplied in two components. The B component is a liquid.Remarks: Indicated values apply to vibrated products.In.. |
|||
Bulk Density | 3.15 - 3.25 g/cc | 0.114 - 0.117 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 180 RAPID Dense Vibrating Refractory Castable Description: Vibron 180 Rapid is a low cement castable based on corundum with a special addition to enable a faster heating schedule. The material is supplied in two components. The B component cont.. |
|||
Bulk Density | 3.16 g/cc | 0.114 lb/in³ | |
Chosun Refractories AM10S Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.15 g/cc | 0.114 lb/in³ | |
Chosun Refractories SAL95S Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.15 - 3.30 g/cc | 0.114 - 0.119 lb/in³ | |
Chosun Refractories SSN-787N Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.15 g/cc | 0.114 lb/in³ | |
Chosun Refractories AM10L Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.15 - 3.25 g/cc | 0.114 - 0.117 lb/in³ | |
Chosun Refractories CSN-A116 Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.15 - 3.25 g/cc | 0.114 - 0.117 lb/in³ | After drying at 110°C |
Gouda Vuurvast FLUCON 180 Dense Self Flowing Refractory Castable Description: Flucon 180 is a self flowing castable based on white fused Alumina. This castable is applied at severe thermal conditions and or severe slag attack.Remarks: These values apply to cast p.. |