Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 185 - 215 MPa @Temperature 1600 °C |
26800 - 31200 psi @Temperature 2910 °F |
Cold Crushing Strength |
Gouda Vuurvast FLUCON 180 Dense Self Flowing Refractory Castable Description: Flucon 180 is a self flowing castable based on white fused Alumina. This castable is applied at severe thermal conditions and or severe slag attack.Remarks: These values apply to cast p.. |