Polymer Property : Thermal Conductivity = 15.3 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 2.00 - 2.20 W/m-K

@Temperature 100 °C
13.9 - 15.3 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURASBOND 85 Moldable Refractory Material
Description: Curasbond 85 is a pouring repairmass, characterized by excellent resistance to aluminum and rapid hardening. The product is supplied in two components: a dry powder and a liquid. It can..
Thermal Conductivity 1.80 - 2.20 W/m-K

@Temperature 100 °C
12.5 - 15.3 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable
Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Rema..
Thermal Conductivity 2.00 - 2.20 W/m-K

@Temperature 1600 °C
13.9 - 15.3 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Gouda Vuurvast FLUCON 180 Dense Self Flowing Refractory Castable
Description: Flucon 180 is a self flowing castable based on white fused Alumina. This castable is applied at severe thermal conditions and or severe slag attack.Remarks: These values apply to cast p..