Material Notes:
Description: Curas 90 PFM ramming mix has outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). In addition, it has a good resistance against thermal shock and corrosive gasses. The product is supplied in two components: a dry powder and a liquid. Curas 90 PFM is applied in the hydrocarbon processing industry.Remarks: The stated chemical composition and physical properties represent average values.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
After drying at 110°C
Mechanical Properties Metric English Comments
Compressive Strength 85.0 - 95.0 MPa

@Temperature 100 °C
12300 - 13800 psi

@Temperature 212 °F
Cold Crushing Strength
120 - 140 MPa

@Temperature 1600 °C
17400 - 20300 psi

@Temperature 2910 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.19 - 1.39 W/m-K

@Temperature 1600 °C
8.26 - 9.65 BTU-in/hr-ft²-°F

@Temperature 2910 °F
1.23 - 1.43 W/m-K

@Temperature 600 °C
8.54 - 9.92 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.25 - 1.45 W/m-K

@Temperature 100 °C
8.68 - 10.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1850 °C
3360 °F
Shrinkage -1.10 - 0.900 %

@Temperature 1600 °C
-1.10 - 0.900 %

@Temperature 2910 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 90 %
90 %
Fe2O3 0.15 %
0.15 %
P2O5 3.0 %
3.0 %
SiO2 6.0 %
6.0 %
Descriptive Properties Value Comments
Bonding Type chemical/ceramic
Material Consumption per 1 m3 2900 kg
Segercone 40