Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.23 W/m-K @Temperature 650 °C |
8.54 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast B 1 Dense Refractory Brick Description: B 1 is a fireclay quality for general applications up to 1350°CRemarks: This data represents average values, obtained from samples that were cut from standard bricks.Information prov.. |
|||
Thermal Conductivity | 1.23 - 1.43 W/m-K @Temperature 1300 °C |
8.54 - 9.92 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURAS 85 PD REPAIR Moldable Refractory Material Description: Curas 85 PD Repair is a phosphate bonded moldable based on sintered bauxite. It has been specially developed for aluminum melting and holding furnaces. However, it can be applied on any.. |
|||
Thermal Conductivity | 1.23 - 1.43 W/m-K @Temperature 600 °C |
8.54 - 9.92 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURAS 90 PF Moldable Refractory Material Description: Curas 90 PF ramming mix with outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). The product is supplied in two components: a dry powder and a liquid. Curas 90 PF i.. |
|||
Thermal Conductivity | 1.23 - 1.43 W/m-K @Temperature 600 °C |
8.54 - 9.92 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURAS 90 PF REPAIR Moldable Refractory Material Description: Curas 90 PF Repair ramming mix is especially developed for repairing purposes of Curas 90 PF linings. The product is supplied in two components: a dry powder and a liquid. Detailed inst.. |
|||
Thermal Conductivity | 1.23 - 1.43 W/m-K @Temperature 600 °C |
8.54 - 9.92 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURAS 90 PFM Moldable Refractory Material Description: Curas 90 PFM ramming mix has outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). In addition, it has a good resistance against thermal shock and corrosive gasses. T.. |
|||
Thermal Conductivity | 1.23 - 1.33 W/m-K @Temperature 600 °C |
8.54 - 9.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro.. |
|||
Thermal Conductivity | 1.23 - 1.33 W/m-K @Temperature 600 °C |
8.54 - 9.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib.. |
|||
Thermal Conductivity | 1.23 - 1.33 W/m-K @Temperature 600 °C |
8.54 - 9.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide.. |
|||
Thermal Conductivity | 1.23 - 1.43 W/m-K @Temperature 1300 °C |
8.54 - 9.92 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURAS 90 SPF Moldable Refractory Material Description: Curas 90 S PF is a moldable which is characterized by its outstanding abrasion resistance (acc. to ASTM C-704: < 3 cc). This material is supplied as a powder which only has to be mixed .. |
|||
Thermal Conductivity | 1.23 - 1.33 W/m-K @Temperature 600 °C |
8.54 - 9.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi.. |