Physical Properties Metric English Comments
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 85 PD Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This phosphate bonded material based on corundum and bauxite has a very go..
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 90 PFM Moldable Refractory Material
Description: Curas 90 PFM ramming mix has outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). In addition, it has a good resistance against thermal shock and corrosive gasses. T..
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
After drying at 110°C
Gouda Vuurvast FLUCON 150 Dense Self Flowing Refractory Castable
Description: Flucon 150 is a self-flowing low cement castable based on sintered bauxite.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 135 Dense Vibrating Refractory Castable
Description: Vibron 135 is a vibrating castable, specially fit for the production of prefab elements. The very low cement content (1%) and the abrasion resistant spinel grains give this material exc..
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 150 Al RAPID Dense Vibrating Refractory Castable
Description: Vibron 150 Al Rapid is a vibrating low cement castable resistant to liquid aluminum metal. Due to a special additive a relatively high heating rate is possible.Remarks: These values app..
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 150 Dense Vibrating Refractory Castable
Description: Vibron 150 is a low cement castable based on sintered bauxite.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 85 PD GM Moldable Refractory Material
Description: This material is supplied as a dry powder and can be gunned. This phosphate bonded material based on corundum and bauxite has a very good resistance against slag attack or liquid alumin..
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
Chosun Refractories BATN-8 Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
Chosun Refractories CSN-309NM,Insert Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
Chosun Refractories CUN-810 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).