Thermal Properties Metric English Comments
Thermal Conductivity 1.23 - 1.43 W/m-K

@Temperature 1300 °C
8.54 - 9.92 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURAS 85 PD REPAIR Moldable Refractory Material
Description: Curas 85 PD Repair is a phosphate bonded moldable based on sintered bauxite. It has been specially developed for aluminum melting and holding furnaces. However, it can be applied on any..
Thermal Conductivity 1.23 - 1.43 W/m-K

@Temperature 600 °C
8.54 - 9.92 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 90 PF Moldable Refractory Material
Description: Curas 90 PF ramming mix with outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). The product is supplied in two components: a dry powder and a liquid. Curas 90 PF i..
Thermal Conductivity 1.23 - 1.43 W/m-K

@Temperature 600 °C
8.54 - 9.92 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 90 PF REPAIR Moldable Refractory Material
Description: Curas 90 PF Repair ramming mix is especially developed for repairing purposes of Curas 90 PF linings. The product is supplied in two components: a dry powder and a liquid. Detailed inst..
Thermal Conductivity 1.23 - 1.43 W/m-K

@Temperature 600 °C
8.54 - 9.92 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 90 PFM Moldable Refractory Material
Description: Curas 90 PFM ramming mix has outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). In addition, it has a good resistance against thermal shock and corrosive gasses. T..
Thermal Conductivity 1.33 - 1.43 W/m-K

@Temperature 100 °C
9.23 - 9.92 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 160 H GS (R) Dense Vibrating Refractory Castable
Description: Vibron 160 H GS (R) is a pumpable low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock-, corrosion- and abrasion resista..
Thermal Conductivity 1.23 - 1.43 W/m-K

@Temperature 1300 °C
8.54 - 9.92 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURAS 90 SPF Moldable Refractory Material
Description: Curas 90 S PF is a moldable which is characterized by its outstanding abrasion resistance (acc. to ASTM C-704: < 3 cc). This material is supplied as a powder which only has to be mixed ..