Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.19 - 1.39 W/m-K

@Temperature 1600 °C
8.26 - 9.65 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Gouda Vuurvast CURAS 90 PF Moldable Refractory Material
Description: Curas 90 PF ramming mix with outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). The product is supplied in two components: a dry powder and a liquid. Curas 90 PF i..
Thermal Conductivity 1.19 - 1.39 W/m-K

@Temperature 1600 °C
8.26 - 9.65 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Gouda Vuurvast CURAS 90 PF REPAIR Moldable Refractory Material
Description: Curas 90 PF Repair ramming mix is especially developed for repairing purposes of Curas 90 PF linings. The product is supplied in two components: a dry powder and a liquid. Detailed inst..
Thermal Conductivity 1.19 - 1.39 W/m-K

@Temperature 1600 °C
8.26 - 9.65 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Gouda Vuurvast CURAS 90 PFM Moldable Refractory Material
Description: Curas 90 PFM ramming mix has outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). In addition, it has a good resistance against thermal shock and corrosive gasses. T..