Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 85.0 MPa @Strain 5 % |
12300 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Compressive Strength | 85.0 MPa @Strain 5 % |
12300 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data) This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie.. |
|||
Compressive Strength | 85.0 MPa @Strain 5 % |
12300 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data) Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr.. |
|||
Compressive Strength | 85.0 - 95.0 MPa @Temperature 100 °C |
12300 - 13800 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURAS 90 PF Moldable Refractory Material Description: Curas 90 PF ramming mix with outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). The product is supplied in two components: a dry powder and a liquid. Curas 90 PF i.. |
|||
Compressive Strength | 85.0 - 95.0 MPa @Temperature 100 °C |
12300 - 13800 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURAS 90 PFM Moldable Refractory Material Description: Curas 90 PFM ramming mix has outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). In addition, it has a good resistance against thermal shock and corrosive gasses. T.. |
|||
Compressive Strength | 85.0 - 95.0 MPa @Temperature 1300 °C |
12300 - 13800 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 135 Dense Vibrating Refractory Castable Description: Vibron 135 is a vibrating castable, specially fit for the production of prefab elements. The very low cement content (1%) and the abrasion resistant spinel grains give this material exc.. |
|||
Compressive Strength | 85.0 - 95.0 MPa @Temperature 100 °C |
12300 - 13800 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 150 G Dense Vibrating Refractory Castable Description: Vibron 150 G is a low cement castable based on sintered South-American bauxite. Especially suited for direct contact with liquid aluminum metal.Remarks: Indicated values apply to vibrat.. |
|||
Compressive Strength | 85.0 - 95.0 MPa @Temperature 100 °C |
12300 - 13800 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 180 T Dense Vibrating Refractory Castable Description: Vibron 180 T is a low cement castable, based on tabular alumina.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |