Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.24 GPa | 469 ksi | ASTM D790 |
Lendell Parapet PMMA, High Flow |
|||
Flexural Modulus | 3.24 GPa @Thickness 3.20 mm |
469 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Flexural Modulus | 3.23 GPa | 469 ksi | ASTM D790 |
Global GP-110 High Impact Polystyrene High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys |
|||
Flexural Modulus | 3.24 GPa @Thickness 3.20 mm |
469 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® LW5102F PBT+PC+GF10% Description: Injection Molding, PBT+PC+GF10%, Low Warpage, Flame RetardantApplication: IT/OA, E&E (Switch)CAS No. 9003-01-04, 68928-70-1, 65997-17-3, 24968-12-5, 103598-77-2 and 1309-64-4Information.. |
|||
Flexural Modulus | 3.24 GPa @Thickness 3.20 mm |
469 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP2102 PC+GF10% Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 3.24 GPa @Temperature 23.0 °C |
469 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene GP110 Polystyrene APPLICATIONS: EXTRUSION SHEET, HOUSEHOLD PRODUCTS VACUUM SHEET , FOOD PACKAGING, TOY, SANITARY WARE, etc. |
|||
Flexural Modulus | 3.24 GPa | 469 ksi | ASTM D790 |
Samyang Tribit® 1500G15K PBT, Reinforced Impact Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G15K is a reinforced, impact grade.Appl.. |
|||
Flexural Modulus | 3.24 GPa | 469 ksi | ASTM D790 |
Cheng Yu Plastic E500G20 PC/PET, 20% Glass Fiber |