Material Notes:
ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be injection molded, blow molded, and extruded. In compliance with FDA CFR 177.105, 177.1680, and 177.2600 requirementsInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Strength 34.0 MPa
4930 psi
ASTM D412
Tensile Strength, Yield 10.0 MPa

@Strain 50.0 %
1450 psi

@Strain 50.0 %
ASTM D412
12.0 MPa

@Strain 100 %
1740 psi

@Strain 100 %
ASTM D412
24.0 MPa

@Strain 300 %
3480 psi

@Strain 300 %
ASTM D412
Elongation at Break 470 %
470 %
ASTM D412
Tear Strength 110 kN/m
628 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 60
60
ASTM D1044(Taber) H-22
Compression Set 30 %

@Temperature 23.0 °C,
Time 79200 sec
30 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
75 %

@Temperature 70.0 °C,
Time 79200 sec
75 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395