Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 34.0 MPa | 4930 psi | ASTM D412 |
GRECO ISOTHANE 1095AF Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject.. |
|||
Tensile Strength | 34.0 MPa | 4930 psi | ASTM D412 |
GRECO ISOTHANE 3080A Polyether TPU Resin ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod.. |
|||
Tensile Strength | 34.0 MPa | 4930 psi | ASTM D412 |
GRECO ISOTHANE 1080A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength | 34.0 MPa | 4930 psi | ASTM D412 |
Teknor Apex Laripur® LPR 9060HFM Thermoplastic Polyurethane Features: - Excellent performance under extreme and aggressive environments
- Superior abrasion and cut resistance
- Resistance to chemical, microbial attack and hydrolysis
- Excellent flexibility a.. |
|||
Tensile Strength | 34.0 MPa | 4930 psi | ASTM D882-80, Method A - 100% |
DuPont™ Tedlar® SP TTR10SH9 Clear Polyvinyl Fluoride Film Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistance, and ease of cleaning ex.. |
|||
Tensile Strength | 34.0 MPa | 4930 psi | ASTM D882-80, Method A - 100% |
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film Transparent, Medium Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resista.. |
|||
Tensile Strength | 34.0 MPa | 4930 psi | ISO 527 |
BASF Ecoflex® 1200 F Blend Biodegradable Polyester Description: A flexible plastic designed for film extrusion and extrusion coating. Ecoflex® F Blend 1200 comes closer than any other biodegradable plastic to the processing properties of LDPE and L.. |
|||
Tensile Strength | 34.0 MPa | 4930 psi | Plasticizer conc. in vinyl film 33 phr; ASTM D638 |
BASF Palamoll® 656 Polymeric Plasticizer Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro.. |
|||
Tensile Strength | 34.0 MPa | 4930 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1590 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 34.0 MPa @Strain 300 % |
4930 psi @Strain 300 % |
ISO 37 |
BASF Elastollan S 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |