Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.0 MPa @Strain 100 % |
1740 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 1055DE Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 300 % |
1740 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1090AE Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 100 % |
1740 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 1095AF Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 300 % |
1740 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1190A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 300 % |
1740 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 3085AF Polyether TPU Resin ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 300 % |
1740 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 5085A Polyether TPU Resin ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 300 % |
1740 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1080AF Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 300 % |
1740 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1085A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 300 % |
1740 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 2080A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 300 % |
1740 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 3085A Polyether TPU Resin ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 100 % |
1740 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 100 % |
1740 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® EM550 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 100 % |
1740 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® EL550 55 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 100 % |
1740 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® EL550 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 100 % |
1740 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tensile Strength, Yield | 12.0 MPa @Strain 300 % |
1740 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |