Master Bond MasterSil 710 Silicone Paste Meets MIL Spec

Category Polymer , Thermoset , Silicone
Manufacturer Master Bond Inc.
Trade Name Mastersil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond MasterSil 710 Silicone Paste Meets MIL Spec.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: MasterSil 710 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This product meets the Meets MIL-A- 46146A Type 1 specification. It is non-corrosive, fast setting and has a paste consistency. It can be widely used for many applications, particularly in aerospace and electronics. MasterSil 710 can be used in electronics, for example, for bonding sensitive wires and components. It bonds well to a wide variety of substrates. The rapidity of the cure depends on the thickness of the layer and the humidity; the thicker the layer the slower the cure. MasterSil 710 is serviceable over the broad temperature range of -75°F to +400°F. Its color is translucent.Information provided by MasterBond®
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 35 - 45
35 - 45
Tensile Strength at Break 3.45 - 4.14 MPa
500 - 600 psi
Elongation at Break 550 - 650 %
550 - 650 %
Shear Strength 0.517 - 1.03 MPa
75.0 - 150 psi
Tensile, Al to Al
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -59.4 °C
-75.0 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Dielectric Constant 2.5

@Frequency 60.0 Hz,
Temperature 25.0 °C
2.5

@Frequency 60.0 Hz,
Temperature 77.0 °F
Dielectric Strength 19.7 kV/mm

@Thickness 3.17 mm
500 kV/in

@Thickness 0.125 in
Dissipation Factor 0.0010

@Frequency 60.0 Hz,
Temperature 25.0 °C
0.0010

@Frequency 60.0 Hz,
Temperature 77.0 °F
Processing Properties Metric English Comments
Cure Time 7.02 - 12.0 min
0.117 - 0.200 hour
Tack-free time
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened containers
Descriptive Properties Value Comments
Appearance Translucent