Polymer Property : Tensile Strength, Yield = 1450 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.0 MPa

@Strain 50.0 %
1450 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 1095AF Poly(adipate)ester TPU Resin
ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject..
Tensile Strength, Yield 10.0 MPa

@Strain 300 %
1450 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1185A Poly(adipate)ester TPU Resin
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp..
Tensile Strength, Yield 10.0 MPa

@Strain 100 %
1450 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 3090A Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tensile Strength, Yield 10.0 MPa

@Strain 300 %
1450 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 5080A Polyether TPU Resin
ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro..
Tensile Strength, Yield 10.0 MPa

@Strain 300 %
1450 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1075A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength, Yield 10.0 MPa

@Strain 100 %
1450 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 10.0 MPa

@Strain 100 %
1450 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® EM460 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 10.0 MPa

@Strain 5.00 %
1450 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PL581 58 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 10.0 MPa

@Strain 5.00 %
1450 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PL581 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 10.0 MPa

@Strain 300 %
1450 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® 1180A Polyether Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes...
Tensile Strength, Yield 10.0 MPa

@Strain 100 %
1450 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® 1190A Polyether Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes...
Tensile Strength, Yield 10.0 MPa

@Strain 100 %
1450 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® C-90A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..