Polymer Property : Viscosity = 0.95 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 0.95 cP
0.95 cP
Inherent; ASTM D1243
Formosa Plastics Formolon® 34 PVC
PVC Homopolymer Dispersion Resin F-34 is a medium molecular weight PVC homopolymer dispersion resin which has been developed primarily for use in chemically expanded compound. In expanded systems, t..
Viscosity 0.95 cP
0.95 cP
Inherent; ASTM D5225
Formosa Plastics Formolon® 676 PVC
Homopolymer General Purpose Grade Resin F676 is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered ..
Viscosity 0.95 cP
0.95 cP
Inherent; ASTM D1243
Formosa Plastics Formolon® KVF PVC
PVC Homopolymer Dispersion Resin F-KVF is a medium molecular weight, fine particle PVC homopolymer dispersion which imparts pesudoplastic flow to plastisol in which it is used. Plastisol prepared ut..
Viscosity 0.95 cP
0.95 cP
Inherent; ASTM D5225
Formosa Plastics Formolon® 676H PVC
Homopolymer General Purpose Grade Resin F676H is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered..