Polymer Property : Particle Mesh Size = 40 Mesh Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Mesh Size 40 Mesh
40 Mesh
Traces; PVCH/QCD/3514
Reliance Industries 60-11 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications:Recommended:Rigid extrusionRigid injectionRigid calenderingCan be used:Blow molding
Particle Mesh Size 40 Mesh
40 Mesh
Traces; PVCH/QCD/3514
Reliance Industries 67-01 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications:Recommended:Rigid extrusion.Can be used:rigid injection.
Particle Mesh Size 40 Mesh
40 Mesh
Traces; PVCH/QCD/3514
Reliance Industries 57-11 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications: Rigid injectionRigid extrusionRigid calenderingblow molding
Particle Mesh Size 40 Mesh
40 Mesh
20.2% retained
Imerys G-20 HP Feldspar
G-20 HP Feldspar is a high potassium aluminium silicate ground to 200 mesh for ceramic applications. G-20HP offers high potassium content and low iron oxide per unit of alumina.Information provided ..
Particle Mesh Size 40 Mesh
40 Mesh
0.3% retained
Imerys G-40 HP Feldspar
G-40 HP fledpsar is a high potassium aluminium silicate ground to 200 mesh for ceramic applications. G-40 HP offers high potassium content and low iron oxide per unit of alumina.Information provided..
Particle Mesh Size 40 Mesh
40 Mesh
55.8% retained; U.S. Sieve
Imerys Minsilsparâ„¢ 1 Feldspar
Minsilspar 1 is a feldspathic sand (sandspar).Information provided by Imerys
Particle Mesh Size 40 Mesh
40 Mesh
99.9% min; ASTM D1921
Westlake 1185 PVC
Westlake PVC 1185 resin is a low molecular weight resin with excellent clarity designed for applications such as blow molding or where high plasticizer uptake is required.Information provided by Wes..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% min; ASTM D1921
Westlake 1195 PVC
Westlake PVC 1195 resin is a low molecular weight resin designed for rigid injection molding, calendering, sheet extrusion, and blow molding.Information provided by Westlake Chemical Corporation
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; ASTM D1921B
Formosa Plastics Formolon® 113 PVC
PVC Copolymer Suspension Resin F-113 has been developed primarily to meet the processing requirements of the vinyl composition tile (VCT) manufacturers. In addition to vinyl floor tile industry, F-1..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; ASTM D1921B
Formosa Plastics Formolon® 165 PVC
PVC Copolymer Suspension Resin F-165 has been developed primarily to meet the processing requirements of the vinyl composition tile (VCT) manufacturers. In addition to vinyl floor tile industry, F-1..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; ASTM D1921B
Formosa Plastics Formolon® 186 PVC
PVC Copolymer Suspension Resin F-186 is a medium molecular vinyl chloride/vinyl acetate copolymer suspension resin. This resin is primarily used in the calendaring and extrusion of rigid film F-186 ..
Particle Mesh Size 40 Mesh
40 Mesh
100% thru; ASTM D1921B
Formosa Plastics Formolon® 260 PVC
PVC Homopolymer Blending Resin F-260 is a fine particle size PVC homopolymer plastisol blending resin. It combines excellent fusion characteristics, low plastisol viscosities as well as lot to lot u..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 608 PVC
PVC Homopolymer General Purpose Grade Resin F608 is a low molecular weight PVC homopolymer of particular interest in rigid applications and has established a deserved reputation for low gels and exc..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 614 PVC
Homopolymer - General Purpose Grade Resin F614 is a medium-low molecular weight PVC homopolymer of particular interest in rigid applications and has established a deserved reputation for low gels an..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 616K PVC
PVC Homopolymer General Purpose Grade Resin F616K is a medium-low molecular weight PVC homopolymer of particular interest in rigid applications and has established a deserved reputation for low gels..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 622 PVC
Homopolymer Pipe Grade Resin F622 is a medium-low molecular weight PVC homopolymer designed primarily for rigid extrusion applications. This product has excellent dry flow characteristics, making i..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 622E PVC
Rigid Extrusion Resin F622E is a medium-low molecular weight PVC designed primarily for rigid extrusion applications. This product has excellent dry flow characteristics, making it desirable for dry..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 622R PVC
Homopolymer General Purpose Grade Resin F622R is a medium-low molecular weight PVC homopolymer of interest in both rigid and flexible applications and has established a deserved reputation for low ..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 622S PVC
Homopolymer Siding Grade Resin F622S is a medium-low molecular weight PVC homopolymer designed primarily for rigid extrusion applications, but it is also suitable for many flexible applications. Thi..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 676 PVC
Homopolymer General Purpose Grade Resin F676 is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered ..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 680 PVC
Homopolymer General Purpose Grade Resin F680 is especially suited for processing from powder blends due to its ability to rapidly absorb plasticizers regardless of molecular weight. In addition, thi..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 690 PVC
Homopolymer General Purpose Grade Resin F690 is especially suited for processing from powder blends due to its ability to rapidly absorb plasticizers regardless of molecular weight. In addition, thi..
Particle Mesh Size 40 Mesh
40 Mesh
90-100%; US std sieve
Zeon Chemicals Zealloy® 1422 Modifier for Thermoplastics
Zealloy 1422 is a copolymer of butadiene and acrylonitrile of medium oil resistance. It is furnished as a finely-divided powder. Sufficient antioxidant is added during manufacture for normal storage..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 622F PVC
Homopolymer Film Grade Resin F622F is a medium molecular weight PVC homopolymer suitable for both rigid extrusion applications and it is suitable for many flexible applications. This product has goo..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 680H PVC
Homopolymer General Purpose Grade Resin F680H is especially suited for processing from powder blends due to its ability to rapidly absorb plasticizers regardless of molecular weight. In addition, th..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 680M PVC
Homopolymer General Purpose Grade Resin F680M is a medium molecular weight PVC homopolymer suitable for both rigid and flexible applications and is low in gels and finds acceptance in calendered fil..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
Formosa Plastics Formolon® 685 PVC
Homopolymer General Purpose Grade Resin F685 is especially suited for processing from powder blends due to its ability to absorb plasticizers regardless of molecular weight. In addition, this produc..
Particle Mesh Size 40 Mesh
40 Mesh
91.0% passing, dry
CIMBAR Suspengel™ 16 High Purity Bentonite, Industrial Grade
Suspengel products are manufactured from the highest quality Western Bentonite reserves. Suspengel products are easy to disperse thixotropes with excellent suspension properties. Strict process co..
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; ASTM D1921B
Formosa Plastics Formolon® 172 PVC
PVC Copolymer Suspension Resin F-172 is a medium molecular vinyl chloride/vinyl acetate copolymer suspension resin. This resin is primarily used in the calendaring and extrusion of rigid film F-172 ..
Particle Mesh Size 40 - 50 Mesh
40 - 50 Mesh
US Sieve
Potters Industries A-Series P-0170 Soda-Lime Silica Technical Quality Solid Glass Spheres
Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil..