Polymer Property : Relative Viscosity = 2.27 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Relative Viscosity 2.27 cP
2.27 cP
Formosa Plastics Formolon® 676 PVC
Homopolymer General Purpose Grade Resin F676 is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered ..
Relative Viscosity 2.27 cP
2.27 cP
Formosa Plastics Formolon® 676H PVC
Homopolymer General Purpose Grade Resin F676H is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered..