Material Notes:
Features: Good clarity and impact resistance. Product does not contain animal derived components.Applications: Injection molding - durable goodsInformation provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 62
62
ASTM D785
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Yield 17 %
17 %
ASTM D638
Flexural Modulus 0.869 GPa
126 ksi
Tangent; ASTM D790
Izod Impact, Notched 3.20 J/cm
5.99 ft-lb/in
ASTM D256
Impact Test 17.6 J

@Temperature 23.0 °C
13.0 ft-lb

@Temperature 73.4 °F
Multi-Axial, Ductile; ASTM D3763
22.0 J

@Temperature 0.000 °C
16.2 ft-lb

@Temperature 32.0 °F
Multi-Axial, Ductile; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C
172 °F
ASTM D648
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 3.1a and 3.2c