Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)  (discontinued **)

Category Polymer , Thermoset , Vinyl Ester , Vinyl Ester Sheet Molding Compound
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
#1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resistant and blended for toughness. The raw materials used in the manufacture of this resin are listed as acceptable in FDA regulatory Title 21 CFR 177.2420 for repeated use in contact with food subject to compliance with the prescribed limitation of that regulation.Performance:Excellent corrosion resistanceExcellent impact strengthHigh tensile elongationFDA applicationProperties listed typical cured casting, catalyzed with 1% BPO, cured two hours at 160°F then one hour at 200°F, post cured two hours at 280°F. See also: "Vinyl Ester Resin (Laminate Properties)" for information on that application.Can be used for hand lay-up and spray-up, filament winding, flake glass and filled lining and coating compounds. Perfect for repairing tank linings, blistering boat hulls, and fabricating tough all-around parts.Information provided by Fibre Glast Developments Corporation.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Liquid Property
Solids Content 52 %
52 %
Liquid Property
Viscosity 275 cP
275 cP
Liquid Property
Mechanical Properties Metric English Comments
Hardness, Barcol 35
35
ASTM D2538
Tensile Strength at Break 827 MPa
120000 psi
ASTM D638
Elongation at Break 7.9 %
7.9 %
ASTM D638
Elongation at Yield 4.6 %
4.6 %
ASTM D638
Tensile Modulus 3.72 GPa
540 ksi
ASTM D638
Flexural Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 98.0 °C
208 °F
Deflection Temp; Load not specified; ASTM D648
Flash Point 22.8 - 37.8 °C
73.0 - 100 °F