Physical Properties Metric English Comments
Viscosity 275 cP

@Temperature 40.0 °C
275 cP

@Temperature 104 °F
25% in dimethylacetamide; Internal Method
Solvay Specialty Polymers Veradel® 3600P Polyethersulfone (PESU)  (Unverified Data**)
Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be g..
Viscosity 275 cP

@Temperature 85.0 °C
275 cP

@Temperature 185 °F
Northstar Polymers MSA-030 Polyester Prepolymer
Information provided by Northstar Polymers.
Viscosity 275 cP
275 cP
Solution Viscosity; ASTM D455
Solvay Specialty Polymers Veradel® 3600P Polyethersulfone (PESU)
Veradel® PESU was formerly marketed as Gafone™ PESU. Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They ca..
Viscosity 275 cP
275 cP
Part B
Resinlab® UR3010 Black Polyurethane Potting System
Resinlab™ UR 3010 Black is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro..
Viscosity 275 cP
275 cP
Part B
Resinlab® UR3010 Clear Polyurethane Potting System
Resinlab™ UR 3010 Clear is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro..
Viscosity 275 cP
275 cP
Liquid Property
Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)  (discontinued **)
#1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resista..