Material Notes:
A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closures and sealing gaskets. It can be processed using injection molding, extrusion, blow molding or other melt processing techniques.Key Features: Excellent flex fatigue resistance; Excellent ozone resistance; May be used in contact with non-fatty foods as closure sealing gaskets in accordance with provisions of 21 CFR 177.1210 under the Federal Food, Drug and Cosmetic Act; Complies with 21 CFR 177.2600 "Rubber Articles Intended for Repeated Use"Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding, extrusion, or blow molding. For extrusion, a general purpose screw with a compression ratio of 2.5 to 3.0 is recommended. Material can be recycled. VYRAM rubber is incompatible with acetal and PVC.Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
TPE-0105 (ASTM D792)
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
5 Second; TPE-0169 (ASTM D 2240)
Tensile Strength, Ultimate 3.60 MPa
522 psi
TPE-0153 (ASTM D 412)
Elongation at Break 450 %
450 %
TPE-0153 (ASTM D 412)
100% Modulus 0.00170 GPa
0.247 ksi
TPE-0153 (ASTM D 412)
Graves Tear Strength 20.0 kN/m
114 pli
TPE-0056 (ASTM D 624)
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
TPE-0089 (ASTM D 746)
Processing Properties Metric English Comments
Processing Temperature 177 - 232 °C
351 - 450 °F
Drying Temperature 82.0 °C
180 °F
Desiccant drying for 3 hours recommended
Dry Time 3 hour
3 hour