ExxonMobil LLDPE LL 8460.29 Linear Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Exxon Chemical
Trade Name LLDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LLDPE LL 8460.29 Linear Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance of processability, stiffness and low temperature toughness. Availability: Latin America, North America and South America Additive: Stabilizer: YesLong Term UV-15 Applications: Agricultural TanksChemical Storage TanksLarge Size Playground EquipmentPalletsPotable Water TanksSeptic TanksInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.938 g/cc
0.0339 lb/in³
ExxonMobil method
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693B
ESCR 10% Igepal® 150 hour
150 hour
F50; ASTM D1693B
Melt Flow 3.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.9 MPa
2600 psi
2.0 in/min; ASTM D638
Elongation at Yield 20 %
20 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 758 MPa
110000 psi
ASTM D638
Impact Test 94.9 J

@Thickness 3.17 mm,
Temperature -40.0 °C
70.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
258 J

@Thickness 6.35 mm,
Temperature -40.0 °C
190 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
Thermal Properties Metric English Comments
Melting Point <= 261 °C
<= 502 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 62.2 °C
144 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 38.9 °C
102 °F
ASTM D648