Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 758 MPa | 110000 psi | ASTM D790B |
ExxonMobil HDPE HD 6601.29 High Density Polyethylene Copolymer Resin Product Description: HD 6601 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance... |
|||
Flexural Modulus, 1% Secant | 758 MPa | 110000 psi | Product Description: LL 6407 is a narrow molecular |
ExxonMobil LL 6407.67 Injection Molding Resin L Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processa.. |
|||
Flexural Modulus, 1% Secant | 758 MPa | 110000 psi | ASTM D638 |
ExxonMobil LLDPE LL 6407.67 Linear Low Density Polyethylene Resin Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processabi.. |
|||
Flexural Modulus, 1% Secant | 758 MPa | 110000 psi | ASTM D790 |
ExxonMobil LLDPE LL 8446.21 Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 8446 is a linear low density butane copolymer designed to offer excellent processability, whiteness, and fast grinding rate. This UV stabilized resin is ideally suited for ap.. |
|||
Flexural Modulus, 1% Secant | 758 MPa | 110000 psi | ASTM D638 |
ExxonMobil LLDPE LL 8450.31 Linear Low Density Polyethylene Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
Flexural Modulus, 1% Secant | 758 MPa | 110000 psi | ASTM D638 |
ExxonMobil LLDPE LL 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Flexural Modulus, 1% Secant | 758 MPa | 110000 psi | ASTM D638 |
ExxonMobil LLDPE LLP 8450.31 Linear Low Density Polyethylene Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
Flexural Modulus, 1% Secant | 758 MPa | 110000 psi | ASTM D638 |
ExxonMobil LLDPE LLP 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Flexural Modulus, 1% Secant | 758 MPa | 110000 psi | ASTM D790A |
Dow DS6D21 Polypropylene Random Copolymer Resin OverviewConsistent processabilityHigh clarity and glossComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDOW DS6D21 Polypropylene Resin is intended for use in case film processes. It is particularly su.. |
|||
Flexural Modulus, 1% Secant | 760 MPa | 110000 psi | ASTM-D790 |
Braskem ML3601U LLDPE Rotomolding Polyethylene The resin ML3601U is a linear low-density polyethylene, 1-hexene based, with excellent environmental stress cracking resistance and high impact strength. It contains long term UV8 stabilization and .. |