Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 62.2 °C | 144 °F | ASTM D648 |
LyondellBasell Alathon® H4262 High Density Polyethylene, Injection Molding Grade
(discontinued **) ApplicationsAlathon H4262 is a high-flow resin that exhibits very good cold temperature impact performance, optimum processing and thermal stability, with good color and organoleptic properties. Typ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 62.2 °C | 144 °F | ASTM D648 |
ExxonMobil LLDPE LL 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 62.2 °C | 144 °F | ASTM D648 |
ExxonMobil LLDPE LLP 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 62.2 °C | 144 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow UNIVAL™ DMDA-6230 NT 7 High Density Polyethylene Resin (HDPE) Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 62.2 °C | 144 °F | ASTM D648 |
Aclo Accucomp Polyethylene HD0200L High Density |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 62.2 °C | 144 °F | ASTM D648 |
Aclo Accucomp Polypropylene CPO402V Automotive Approved Copolymer Extrusion Grade |