Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LLDPE LL 6301RQ Molding Linear Low Density Polyethylene Resin (European Grade)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Exxon Chemical
Trade Name LLDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LLDPE LL 6301RQ Molding Linear Low Density Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 6301 series are medium flow LLDPE grades, with a relatively molecular weight, resulting in molded articles which are very tough and exhibit excellent environmental stress cracking resistance. When compared to LDPE grades of equivalent density, LL 6301 grades exhibits a higher heat deflection temperature and a significantly greater resistance to long term creep. Availability: Africa & Middle East, Asia Pacific and Europe Additive: CapsCompoundingHousewaresTechnical PartsThreaded ClosuresInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil method
ESCR 10% Igepal® 30 hour

@Temperature 50.0 °C
30 hour

@Temperature 122 °F
ASTM D1693B
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.8 MPa
2000 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Elongation at Yield 20 %
20 %
ASTM D638
Flexural Modulus, 1% Secant 490 MPa
71000 psi
ASTM D790
Izod Impact, Notched (ISO) 39.9 kJ/m²
19.0 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point <= 257 °C
<= 495 °F
Peak Melting Point; ExxonMobil method
Users viewing this material also viewed the following: