Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 490 MPa | 71000 psi | ASTM D790 |
ExxonMobil LLDPE LL 6301RQ Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6301 series are medium flow LLDPE grades, with a relatively molecular weight, resulting in molded articles which are very tough and exhibit excellent environmental stress cra.. |
|||
Flexural Modulus, 1% Secant | 490 MPa | 71000 psi | ASTM D790 |
ExxonMobil LLDPE LL 6301XR Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6301 series are medium flow LLDPE grades, with a relatively molecular weight, resulting in molded articles which are very tough and exhibit excellent environmental stress cra.. |