Polymer Property : Izod Impact, Notched (ISO) = 39.9 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 39.9 kJ/m²
19.0 ft-lb/in²
ISO 180/A
ExxonMobil Exxtral™ BMV 201 Performance Polyolefin
Product Description: A specialty thermoplastic olefin injection molding compound resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for large automotive e..
Izod Impact, Notched (ISO) 39.9 kJ/m²
19.0 ft-lb/in²
ISO 180/A
ExxonMobil Exxtral™ H1725 Performance Polyolefin
Product Description: A specialty thermoplastic olefin compound resin with good flow, cold temperature resistance, high flexural modulus, low CLTE, and excellent paintability for automotive exterior ..
Izod Impact, Notched (ISO) 39.9 kJ/m²
19.0 ft-lb/in²
ISO 180/1A
ExxonMobil LLDPE LL 6301RQ Molding Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6301 series are medium flow LLDPE grades, with a relatively molecular weight, resulting in molded articles which are very tough and exhibit excellent environmental stress cra..
Izod Impact, Notched (ISO) 39.9 kJ/m²
19.0 ft-lb/in²
ISO 180/1A
ExxonMobil LLDPE LL 6301XR Molding Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6301 series are medium flow LLDPE grades, with a relatively molecular weight, resulting in molded articles which are very tough and exhibit excellent environmental stress cra..