ExxonMobil LL 5252.09 Compounding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Compounding Resin
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LL 5252.09 Compounding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending with pigments, slip and antiblock additives.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoProcessing Aid: No Thermal Stabilizer: YesApplications: Masterbatch Base Resin Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ExxonMobil Method
Melt Flow 52 g/10 min

@Load 2.16 kg,
Temperature 190 °C
52 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
15s; ASTM D2240
Tensile Strength at Break 15.4 MPa
2230 psi
Elongation at Break 40 %
40 %
ASTM D638
1% Secant Modulus 448 MPa
65000 psi
ASTM D790
Izod Impact, Notched 4.43 J/cm
8.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 122 °C
252 °F
Peak Melting Temperature; ExxonMobil Method
Brittleness Temperature -76.1 °C
-105 °F
ASTM D746
Descriptive Properties Value Comments
Features Thermal Stabilizer