Polymer Property : Izod Impact, Notched = 8.30 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.43 J/cm
8.30 ft-lb/in
ASTM D-256
PlastiComp Velocity® LGF60-PA66 High Flow Nylon 66, 60% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Izod Impact, Notched 4.43 J/cm
8.30 ft-lb/in
ASTM D256-56
Rotuba 880 Ethyl Cellulose
Data provided by the manufacturer.
Izod Impact, Notched 4.43 J/cm
8.30 ft-lb/in
ASTM D256
Teknor Apex Sinvicomp DBS 2006 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Ultra High Impact Resistance Uses: Piping Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex
Izod Impact, Notched 4.43 J/cm
8.30 ft-lb/in
ASTM D256
Eastman Tenite Propionate 380A2R30015 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Izod Impact, Notched 4.43 J/cm
8.30 ft-lb/in
ASTM D256
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Izod Impact, Notched 4.43 J/cm
8.30 ft-lb/in
ASTM D256
ExxonMobil LL 5252.09 Compounding Resin
Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending ..
Izod Impact, Notched 4.43 J/cm
8.30 ft-lb/in
ASTM D256
ExxonMobil LLDPE LL 5252.09 Linear Low Density Polyethylene Resin
Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending ..
Izod Impact, Notched 4.43 - 5.00 J/cm
8.30 - 9.37 ft-lb/in
Average value: 4.81 J/cm Grade Count:3
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m..